C276 is a
nickel-molybdenum-chromium superalloy with an addition of tungsten designed to
have excellent corrosion resistance in a wide range of severe environments. The
high chromium, molybdenum and tungsten contents make the alloy especially
resistant to pitting and crevice corrosion in reducing environments while
chromium conveys resistance to oxidizing media. The low carbon content
minimizes carbide precipitation during welding to maintain corrosion resistance
in as-welded structures.
Alloy C276 is resistant to the formation of grain boundary precipitates in the
weld heat-affected zone, thus making it suitable for most chemical process
application in an as welded conditions. Alloy C276 is widely used in the most
severe environments such as mixed acid chemical processing, pollution control,
pulp and paper production, industrial and municipal waste treatment, and
recovery of sour oil and gas.
Mechanical Properties
Temper |
Annealed |
|
Tensile Rm |
100 |
ksi (min) |
Tensile Rm |
690 |
MPa (min) |
R.p. 0.2% Yield |
41 |
ksi (min) |
R.p. 0.2% Yield |
290 |
MPa (min) |
Elongation (2” or 4D gl) |
40 |
% (min) |
Physical Properties (Room Temperature)
Specific Heat (0-100°C) |
427 |
J.kg-1.°K-1 |
Thermal Conductivity |
9.4 |
W.m -1.°K-1 |
Thermal Expansion |
11.2 |
μm/μm/°C |
Modulus Elasticity |
221 |
GPa |
Electrical Resistivity |
1.30 |
Ohm-cm |
Density |
8.89 |
g/cm3 |
Chemical Composition (% by weight)
|
||
Element |
Min |
Max |
C |
- |
0.02 |
Si |
- |
0.08 |
Mn |
- |
1 |
P |
- |
0.03 |
S |
- |
0.3 |
Co |
- |
2.5 |
Fe |
4 |
7 |
Cr |
14.5 |
16.5 |
Cu |
3 |
4.5 |
Mo |
15 |
17 |
V |
- |
0.35 |
Ni |
Balance |